dc.description.abstract | Hot Isostatic Pressing (HIP) is a thermomechanical post-processing technique widely used in Additive
Manufacturing parts to reduce internal defects, such as entrapped-gas-pores or lack-of-fusion, which have a great
influence on the mechanical and fatigue properties of the material. In this paper, the effect of a non-conventional
HIP-cycle on the fatigue behavior of a Ti-6Al-4V alloy manufactured by Selective Laser melting (SLM) is studied.
The HIP-cycle examined in this study is carried out at pressure of 200 MPa and a temperature of 850 ◦C for 2 h.
Moreover, the cooling process is faster than that obtained from conventional furnace cooling rates, with the aim
to limit the microstructural coarsening effects that affect the fatigue behavior. For the study, an extensive
experimental fatigue program was carried out which included a first batch of SLM specimens tested under as-built
conditions, a second batch of SLM specimens subjected to the present HIP process, and a third batch of specimens
of a reference wrought processed material obtained by rolling and annealing processes. The microstructure of the
material, before and after HIPping, is analyzed and a fractographic analysis is carried out to study the mechanism
of crack initiation and its relation to the fatigue behavior. The results show that the present HIP-process allows
for very good material densification, a microstructure that shows minimal coarsening effects, and good fatigue
properties comparable to the conventional wrought processed material. | en |
dc.description.sponsorship | The authors gratefully acknowledge financial support from the Junta de Castilla y León (Spain) through grant BU-002-P20, co-financed by FEDER funds. | en |
dc.format.mimetype | application/pdf | |
dc.language.iso | eng | es |
dc.publisher | Elsevier | en |
dc.relation.ispartof | International Journal of Fatigue. 2022, V. 163, 107097 | en |
dc.rights | Atribución 4.0 Internacional | * |
dc.rights.uri | http://creativecommons.org/licenses/by/4.0/ | * |
dc.subject | Ti-6A1-4V | en |
dc.subject | Hot isostatic pressing | en |
dc.subject | Selective Laser Melting | en |
dc.subject | Fatigue behavior | en |
dc.subject | Microstructure | en |
dc.subject.other | Ingeniería civil | es |
dc.subject.other | Civil engineering | en |
dc.title | Effect of HIP post-processing at 850 °C/200 MPa in the fatigue behavior of Ti-6Al-4V alloy fabricated by Selective Laser Melting | en |
dc.type | info:eu-repo/semantics/article | es |
dc.rights.accessRights | info:eu-repo/semantics/openAccess | es |
dc.relation.publisherversion | https://doi.org/10.1016/j.ijfatigue.2022.107097 | es |
dc.identifier.doi | 10.1016/j.ijfatigue.2022.107097 | |
dc.relation.projectID | info:eu-repo/grantAgreement/Junta de Castilla y León//BU-002-P20//Optimización de las técnicas de post-procesado para la mejora de propiedades mecánicas y de fatiga en componentes realizados mediante fabricación aditiva/ | es |
dc.journal.title | International Journal of Fatigue | en |
dc.volume.number | 163 | es |
dc.type.hasVersion | info:eu-repo/semantics/publishedVersion | es |